• EI
  • Scopus
  • 食品科学与工程领域高质量科技期刊分级目录第一方阵T1
  • DOAJ
  • EBSCO
  • 北大核心期刊
  • 中国核心学术期刊RCCSE
  • JST China
  • FSTA
  • 中国精品科技期刊
  • 中国农业核心期刊
  • CA
  • WJCI
  • 中国科技核心期刊CSTPCD
  • 中国生物医学SinoMed
中国精品科技期刊2020
尹国平, 陈志周, 刘冰. 纳米SiO2改性大豆蛋白/聚乙烯醇复合薄膜的研究[J]. 食品工业科技, 2013, (18): 110-113. DOI: 10.13386/j.issn1002-0306.2013.18.006
引用本文: 尹国平, 陈志周, 刘冰. 纳米SiO2改性大豆蛋白/聚乙烯醇复合薄膜的研究[J]. 食品工业科技, 2013, (18): 110-113. DOI: 10.13386/j.issn1002-0306.2013.18.006
YIN Guo-ping, CHEN Zhi-zhou, LIU Bing. Study on soy protein/polyvinyl alcohol composite films modified by nano-SiO2[J]. Science and Technology of Food Industry, 2013, (18): 110-113. DOI: 10.13386/j.issn1002-0306.2013.18.006
Citation: YIN Guo-ping, CHEN Zhi-zhou, LIU Bing. Study on soy protein/polyvinyl alcohol composite films modified by nano-SiO2[J]. Science and Technology of Food Industry, 2013, (18): 110-113. DOI: 10.13386/j.issn1002-0306.2013.18.006

纳米SiO2改性大豆蛋白/聚乙烯醇复合薄膜的研究

Study on soy protein/polyvinyl alcohol composite films modified by nano-SiO2

  • 摘要: 为增强大豆蛋白/聚乙烯醇(PVA)复合薄膜的综合性能,以薄膜拉伸强度、断裂伸长率、透光率、吸水率为主要评价指标,通过隶属度函数综合评价方法,研究了纳米SiO2对大豆蛋白/聚乙烯醇复合膜性能的影响。实验结果表明:纳米SiO2添加量,分散剂的添加量,pH对膜的性能均有影响。当加入1.0%的SiO2纳米粒子(占大豆蛋白和PVA干重),1.5%的聚乙烯基吡咯烷酮(占纳米粒子干重),膜液的pH控制在4.0时,复合薄膜的综合性能最好,拉伸强度为9.71MPa,断裂伸长率为89.86%,透光率为25.07%,吸水率为48.35%。 

     

    Abstract: To modify the comprehensive properties of soy protein/polyvinyl alcohol (PVA) films, effects of reducing agents on the properties of the films were studied.The tensile strength, elongation, transmittance and water absorption of the films were compared.Furthermore, a vague mathematics model was used to evaluate quality of the films.Experimental results showed that the addition of nano-SiO2, addition of dispersant and pH of film liquid all had effects on the properties of the soy protein/PVA films.And the optimum film-forming conditions were 1.0% SiO2 nanoparticles (based on the dry weight of soy protein and PVA) , 1.5% PVP (based on weight of SiO2 nanoparticles) and pH4.0, then tensile strength, elongation, transmittance and water absorption of the films were 9.71MPa, 89.86%, 25.07%, 48.35%, respectively.

     

/