许磊,张文昌,赵岩,等. 非晶化甲壳素脱乙酰制备高脱乙酰度壳聚糖[J]. 食品工业科技,2021,42(13):216−220. doi: 10.13386/j.issn1002-0306.2020100188.
引用本文: 许磊,张文昌,赵岩,等. 非晶化甲壳素脱乙酰制备高脱乙酰度壳聚糖[J]. 食品工业科技,2021,42(13):216−220. doi: 10.13386/j.issn1002-0306.2020100188.
XU Lei, ZHANG Wenchang, ZHAO Yan, et al. Preparation of Chitosan with High Degree of Deacetylation from Amorphous Chitin[J]. Science and Technology of Food Industry, 2021, 42(13): 216−220. (in Chinese with English abstract). doi: 10.13386/j.issn1002-0306.2020100188.
Citation: XU Lei, ZHANG Wenchang, ZHAO Yan, et al. Preparation of Chitosan with High Degree of Deacetylation from Amorphous Chitin[J]. Science and Technology of Food Industry, 2021, 42(13): 216−220. (in Chinese with English abstract). doi: 10.13386/j.issn1002-0306.2020100188.

非晶化甲壳素脱乙酰制备高脱乙酰度壳聚糖

Preparation of Chitosan with High Degree of Deacetylation from Amorphous Chitin

  • 摘要: 对甲壳素进行超微粉碎处理,通过控制碾磨时间,得到结晶度为80.91%、58.06%、31.94%和8.09%等4种甲壳素细粉,再对其和普通粉碎甲壳素的非均相脱乙酰制备壳聚糖的反应进行对比研究。结果表明,随着甲壳素样品结晶度的降低,在相同的脱乙酰反应条件下制备的壳聚糖的脱乙酰度更高。采用单次碱处理的方式,使用普通粉碎甲壳素得到的壳聚糖脱乙酰度为84%,使用结晶度为31.94%和8.09%的甲壳素细粉,壳聚糖脱乙酰度可达90%以上。动力学研究分析,普通粉碎甲壳素和超微粉碎处理得到的4种甲壳素细粉非均相脱乙酰反应的活化能分别为58.71、47.23、42.30、35.44和31.73 kJ/mol,即反应的活化能随结晶度的降低而降低,表明非晶化处理能增强甲壳素非均相脱乙酰反应活性。

     

    Abstract: By controlling the grinding time, four kinds of chitin powders with crystallinity of 80.91%, 58.06%, 31.94% and 8.09% were obtained by superfine grinding of chitin, then the heterogeneous deacetylation reaction of them and ordinary grinding chitin was comparative studied. The results showed that the degree of deacetylation of the prepared chitosan was increased with the decrease of crystallinity of chitin. Chitosan with high degree of deacetylation (>90%) could be obtained by single alkali treatment by using chitin powder with crystallinity of 31.94% and 8.09%, and the degree of deacetylation chitosan with ordinary grinding chitin was only 84%. According to the kinetic analysis, the activation energies of heterogeneous deacetylation of chitin powder obtained by ordinary grinding and four kinds of chitin powders obtained by superfine grinding were 58.71, 47.23, 42.30, 35.44 and 31.73 kJ/mol, respectively. The activation energy of the reaction decreased with the decrease of crystallinity, which indicated that amorphous treatment could enhance the heterogeneous deacetylation activity of chitin.

     

/